Stencils and openings
Paste is applied through a stencil, usually a laser-cut sheet of stainless steel, with one aperture (opening) per pad. For fine-pitch parts (parts with closely spaced pins), the aperture is slightly smaller than the pad to prevent bridging (solder joining two pads). Large thermal pads (pads that carry heat) may use a grid of smaller openings, which prevents solder from pooling and leaving voids (empty pockets). Stencil thickness, commonly 0.1 to 0.15 mm, sets the paste volume. Use a thicker stencil for big parts that need more solder, and a thinner one for fine pitch. Getting this wrong is a leading cause of assembly defects: too much paste bridges, and too little gives weak or open joints.
Paste, profile and inspection
Paste has a shelf life and a floor life (the time it can stay out of refrigeration). Expired paste solders badly, and nobody can tell by looking. The reflow profile (the oven's ramp, soak, peak and cooling schedule) must match the paste maker's specification and the board's thermal mass (how much heat the board absorbs). After reflow, inspection catches what the profile did not prevent. AOI (automated optical inspection, a camera check) finds visible problems. X-ray finds hidden joints under BGAs (chips with pads underneath) and QFNs (chips with pads around the edge).
How MICA relates to paste
Paste data from the same footprints
MICA generates a paste layer in the Gerber export (the files a factory uses to make the board). It comes from the pads in the footprint data. The pick-and-place file and the BOM (bill of materials, the list of parts to buy) go with it. MICA does not choose your stencil thickness or reflow profile. Those depend on your assembler's process, and your assembler should make that call with the Gerber files in hand.
Paste types: powder size matters
Solder paste is classified by powder particle size. Type 3 (25 to 45 µm, or micrometers) is the general-purpose standard. Type 4 (20 to 38 µm) and Type 5 print finer apertures for 0.4 to 0.5 mm pitch (the spacing between pin centers) and smaller. Finer powder prints smaller deposits more consistently, but it also oxidizes faster and costs more. Match the paste type to your finest pitch. Respect floor life too: paste out of refrigeration has a working window, typically hours to a day depending on type, after which print quality degrades invisibly. Expired paste is a defect source you cannot see until reflow.